System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Flame Retardant
Material Notes:
Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.
Information Provided by E-Polymers Co., Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.27
g/cc
1.27
g/cc
ASTM D792
Linear Mold Shrinkage
0.012
cm/cm
0.012
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength
30.411
MPa
4410.8
psi
ASTM D638
Elongation at Break
30 %
30 %
ASTM D638
Flexural Strength
68.67
MPa
9960
psi
ASTM D790
Flexural Modulus
2.7468
GPa
398.39
ksi
ASTM D790
Izod Impact, Notched
0.412
J/cm
0.771
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
133
°C
271
°F
ASTM D648
Flammability, UL94
V-0
V-0
Processing Properties
Metric
English
Comments
Melt Temperature
170
-
200
°C
338
-
392
°F
Mold Temperature
40.0
-
60.0
°C
104
-
140
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized
Cossa Polimeri ESTAPROP 0540 GFC V0 Flame Retardant Polypropylene, 20% Glass Filled
PEPOLZ054 / 103551
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.