MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MetalTek Bearium® B-10 Bearing Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.

Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mission critical bearings and bushings.

Information provided by MetalTek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 55500 kg
Tensile Strength, Ultimate >= 175 MPa
Tensile Strength, Yield >= 100 MPa
Elongation at Break >= 10 %
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 70 %
Lead, Pb 20 %
Tin, Sn 10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Oilite® Bronze Bearing Alloy - SAE 841
Mueller Dynalloy Alloy 6730 Free cutting bearing bronze (UNS C67300)
Tin Bronze UNS C90300, Copper Casting Alloy
MetalTek NAVY G Cast UNS C90300 Bearing Bronze

NMETEK026 / 18276

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.