MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco MERCON® V Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Beginning with the 1997 model year, Ford introduced a higher performance level ATF with the MERCON V specification. Many Ford automatic transmissions from 1999 on will require a MERCON V fluid. The most notable exceptions are the E40D, 4R100, and CD4E transmissions, which still specify regular MERCON ATF.

Chevron ATF MERCON® is fully approved for MERCON V, as well as DEXRON®-III and MERCON® approved. It provides excellent performance in frigid cold and is formulated to resist viscosity breakdown for long fluid life.

Applications

Chevron Automatic Transmission Fluid MERCON V is designed specifically for use in Ford Motor Compay transmissions that require a MERCON V fluid. The enhanced properties of the MERCON V specification offer premium performance in MERCON or DEXRON-III applications.

Key Words: CPS Number: 226719; MSDS Number: 8061
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.8 °
Brookfield Viscosity 11500 cP
@Temperature -40.0 °C
Viscosity Measurement 194Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 202 SUS
Saybolt Viscosity at 210°F 54 SUS
Kinematic Viscosity at 40°C (104°F) 40 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 8.4 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -45.0 °CASTM D97
Flash Point 196 °CASTM D92
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
Phillips 66 Triton® Heavy Duty ATF Automatic Transmission Fluid
Phillips 66 Kendall® Classic ATF Transmission Fluid
Phillips 66 CVT Fluid Full-Synthetic Transmission Fluid
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid

WCHEV042 / 74657

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.