Physical Properties | Metric | English | Comments |
---|
Density | 1.32 g/cc | 0.0477 lb/in³ |
| 0.743 g/cc @Temperature 150 °C | 0.0268 lb/in³ @Temperature 302 °F |
| 0.863 g/cc @Temperature 140 °C | 0.0312 lb/in³ @Temperature 284 °F |
| 0.939 g/cc @Temperature 130 °C | 0.0339 lb/in³ @Temperature 266 °F |
| 0.998 g/cc @Temperature 120 °C | 0.0361 lb/in³ @Temperature 248 °F |
| 1.049 g/cc @Temperature 110 °C | 0.03790 lb/in³ @Temperature 230 °F |
| 1.093 g/cc @Temperature 100 °C | 0.03949 lb/in³ @Temperature 212 °F |
| 1.133 g/cc @Temperature 90.0 °C | 0.04093 lb/in³ @Temperature 194 °F |
| 1.17 g/cc @Temperature 80.0 °C | 0.0423 lb/in³ @Temperature 176 °F |
| 1.205 g/cc @Temperature 70.0 °C | 0.04353 lb/in³ @Temperature 158 °F |
| 1.237 g/cc @Temperature 60.0 °C | 0.04469 lb/in³ @Temperature 140 °F |
| 1.268 g/cc @Temperature 50.0 °C | 0.04581 lb/in³ @Temperature 122 °F |
| 1.297 g/cc @Temperature 40.0 °C | 0.04686 lb/in³ @Temperature 104 °F |
| 1.325 g/cc @Temperature 30.0 °C | 0.04787 lb/in³ @Temperature 86.0 °F |
| 1.352 g/cc @Temperature 20.0 °C | 0.04884 lb/in³ @Temperature 68.0 °F |
| 1.378 g/cc @Temperature 10.0 °C | 0.04978 lb/in³ @Temperature 50.0 °F |
| 1.404 g/cc @Temperature 0.000 °C | 0.05072 lb/in³ @Temperature 32.0 °F |
Molecular Weight | 134 g/mol | 134 g/mol |
Vapor Pressure | 1.2273 bar | 920.52 torr |
| 0.29647 bar @Temperature -12.2 °C | 222.37 torr @Temperature 10.0 °F |
| 0.39298 bar @Temperature -6.67 °C | 294.76 torr @Temperature 20.0 °F |
| 0.51021 bar @Temperature -1.11 °C | 382.69 torr @Temperature 30.0 °F |
| 0.65500 bar @Temperature 4.44 °C | 491.29 torr @Temperature 40.0 °F |
| 0.82737 bar @Temperature 10.0 °C | 620.58 torr @Temperature 50.0 °F |
| 1.0411 bar @Temperature 15.6 °C | 780.89 torr @Temperature 60.0 °F |
| 1.2893 bar @Temperature 21.1 °C | 967.07 torr @Temperature 70.0 °F |
| 1.586 bar @Temperature 26.7 °C | 1189 torr @Temperature 80.0 °F |
| 1.937 bar @Temperature 32.2 °C | 1453 torr @Temperature 90.0 °F |
| 2.337 bar @Temperature 37.8 °C | 1753 torr @Temperature 100 °F |
| 2.8062 bar @Temperature 43.3 °C | 2104.8 torr @Temperature 110 °F |
| 3.337 bar @Temperature 48.9 °C | 2503 torr @Temperature 120 °F |
| 3.944 bar @Temperature 54.4 °C | 2958 torr @Temperature 130 °F |
| 4.633 bar @Temperature 60.0 °C | 3475 torr @Temperature 140 °F |
| 5.412 bar @Temperature 65.6 °C | 4060 torr @Temperature 150 °F |
| 6.281 bar @Temperature 71.1 °C | 4711 torr @Temperature 160 °F |
| 7.253 bar @Temperature 76.7 °C | 5440 torr @Temperature 170 °F |
| 8.336 bar @Temperature 82.2 °C | 6252 torr @Temperature 180 °F |
| 9.529 bar @Temperature 87.8 °C | 7147 torr @Temperature 190 °F |
| 10.85 bar @Temperature 93.3 °C | 8140 torr @Temperature 200 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Thermal Conductivity | 0.0105 W/m-K @Temperature 0.000 °C | 0.0729 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
| 0.0113 W/m-K @Temperature 10.0 °C | 0.0784 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
| 0.0121 W/m-K @Temperature 20.0 °C | 0.0840 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
| 0.0129 W/m-K @Temperature 30.0 °C | 0.0895 BTU-in/hr-ft²-°F @Temperature 86.0 °F |
| 0.0137 W/m-K @Temperature 40.0 °C | 0.0951 BTU-in/hr-ft²-°F @Temperature 104 °F |
| 0.0145 W/m-K @Temperature 50.0 °C | 0.101 BTU-in/hr-ft²-°F @Temperature 122 °F |
| 0.0154 W/m-K @Temperature 60.0 °C | 0.107 BTU-in/hr-ft²-°F @Temperature 140 °F |
| 0.0163 W/m-K @Temperature 70.0 °C | 0.113 BTU-in/hr-ft²-°F @Temperature 158 °F |
| 0.0172 W/m-K @Temperature 80.0 °C | 0.119 BTU-in/hr-ft²-°F @Temperature 176 °F |
| 0.0183 W/m-K @Temperature 90.0 °C | 0.127 BTU-in/hr-ft²-°F @Temperature 194 °F |
| 0.0194 W/m-K @Temperature 100 °C | 0.135 BTU-in/hr-ft²-°F @Temperature 212 °F |
| 0.0207 W/m-K @Temperature 110 °C | 0.144 BTU-in/hr-ft²-°F @Temperature 230 °F |
| 0.0224 W/m-K @Temperature 120 °C | 0.155 BTU-in/hr-ft²-°F @Temperature 248 °F |
| 0.0246 W/m-K @Temperature 1360 °C | 0.171 BTU-in/hr-ft²-°F @Temperature 2480 °F |
| 0.0282 W/m-K @Temperature 140 °C | 0.196 BTU-in/hr-ft²-°F @Temperature 284 °F |
| 0.0365 W/m-K @Temperature 150 °C | 0.253 BTU-in/hr-ft²-°F @Temperature 302 °F |
| 14.0 W/m-K @Temperature 40.0 °C | 97.2 BTU-in/hr-ft²-°F @Temperature 104 °F |
Melting Point | <= 107 °C | <= 225 °F |
Boiling Point | 15.3 °C | 59.5 °F |