MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M ScotchCal™ 3690E Graphic Film Material
Categories: Polymer; Adhesive; Film

Material Notes: 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small diameter applications. These film materials utilize 3M™ Adhesive 320 which offers high initial tack and excellent adhesion to a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics such as polyethylene.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.00 milAdhesive
 2.00 milFacestock
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 3.6875 pliPolypropylene, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
 5.00 pliChrome, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
 5.00 pliAcrylic Paint, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
 5.00 pliABS Plastic, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
 5.9375 pliAluminum, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
 6.375 pliStainless Steel, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 °CPermanent
 150 °CShort term
Minimum Service Temperature, Air -60.0 °CShort term
 -60.0 °CPermanent
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 10.0 °CApplication
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Type320 High Tenacity Acrylic
LinerYellow Glassine Liner

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 9447 Adhesive Transfer Tape
3M Scotchcal™ 3690LF Graphic Film
3M Scotchcal™ 3690 Graphic Film
3M ScotchCal™ 3698E Graphic Film Material

PMM33730 / 168477

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.