MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Grade 18Ni (250) Maraging Steel, Aged, 75 mm round bar, tested longitudinal
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel; Maraging Steel

Material Notes: Applications: Bearings, Belleville springs, bolts, cannon recoil springs, rocket motor and missiles cases, couplings, load cells, flexures for guidance mechanisms of missiles, helicopter drive shafts, transmission shafts, fan shafts in commercial jet engines, aircraft wing components and forgings, aluminum die casting dies, cold forming dies, plastic molding dies, cores, pins, punches, and trim knees.

Key Words: maraging steels, UNS K92890, ASTM A538 (B), ASTM A579 grade 72
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 491Converted from Rockwell C hardness.
Hardness, Knoop 544Converted from Rockwell C hardness.
Hardness, Rockwell C 50.4
Hardness, Vickers 523Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1750 MPa
Tensile Strength, Yield 1712 MPa
@Strain 0.2 %
RT
Elongation at Break 11 %in gage length of 4.5 times the square root of area.
Reduction of Area 53.4 %
Modulus of Elasticity 190 GPa
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.30Calculated
Shear Modulus 73.0 GPaEstimated from elastic modulus
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000174 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.1 µm/m-°C
@Temperature 21.0 - 480 °C
Thermal Conductivity 25.3 W/m-K
@Temperature 20.0 °C
 25.8 W/m-K
@Temperature 50.0 °C
 27.0 W/m-K
@Temperature 100 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.10 %
Boron, B 0.0030 %
Carbon, C <= 0.030 %
Cobalt, Co 7.5 %
Iron, Fe 68 %As remainder
Manganese, Mn <= 0.10 %
Molybdenum, Mo 4.8 %
Nickel, Ni 18.5 %
Phosphorus, P <= 0.010 %
Silicon, Si <= 0.10 %
Sulfur, S <= 0.010 %
Titanium, Ti 0.40 %
Zirconium, Zr 0.010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Grade 18Ni (250) Maraging Steel, nominal annealed properties
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 510°C (950°F) for 3 hours
AISI Grade 18Ni (250) Maraging Steel, Aged, 150 mm square bar, tested longitudinal
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 1 hour
AISI Grade 18Ni (250) Maraging Steel, Aged, 32 mm round bar, tested longitudinal

M1825D / 7379

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.