MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aurora Plastics TufTech™ GA-1050 PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Application: A UL Bulletinized, VW-1, 105°C rated compound for THHN, THWN, MTW, 1000 volt applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95
@Time 15.0 sec
ASTM D2240
Tensile Strength 19.3 MPaASTM D412
Elongation at Break 300 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 28 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 - 360 °FSuggested Stock

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aurora Plastics GA-1050-OR3-LF PVC
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F
Arkema Lacovyl® PS 1050 PVC
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050

PSEPN081 / 179085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.