MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Lacovyl® PS 1050 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: LACOVYL PS 1050 is a vinyl chloride homopolymer obtained by the suspension polymerization process.

* MAIN CHARACTERISTICS

  • Viscosity index (ISO 1628-2):100 ml/g,(K value:64).

LACOVYL PS 1050 can be incorporated with plastisols based on microsuspension - or emulsion - polymerized PVC to:

  • obtain a lower-cost formulation,
  • reduce and stabilize viscosity in storage,
  • enhance pseudo-plasticity,
  • reduce gloss in surface layers,
  • improve transparency and thermal stability while maintaining equivalent mechanical properties and good low-temperature flexibility,
  • inhibit foaming (Congoleum process). By virtue of its exceptionally fine state of division, it can be used in the thinnest possible layers. It is usable in every type of application, at up to 50 phr in certain cases.

* APPLICATIONS

LACOVYL PS 1050 can be used in all plastisol applications, in the manufacture of materials for:

  • the building industry (floor and wall coverings),
  • the motor industry (artificial leather and mastics),
  • the food industry (closures etc...),
  • morocco-leather goods, footwear (artificial leather), etc..

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Number 100 cm³/g1.00 dl/g
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %Mfr. reports 'Transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aurora Plastics TufTech™ GA-1050 PVC Compound
Aurora Plastics GA-1050-OR3-LF PVC
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050

PZARKG296 / 25590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.