MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based conductive elastomer materials offer excellent resistance to compression set over a wide temperature range, resulting in years of continuous service.

Molded and Extruded

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.45 - 3.95 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 57 - 73ASTM D2240
Tensile Strength at Break >= 175 psiASTM D412
Elongation at Break >= 75 %ASTM D412
Compression Set <= 32 %
@Temperature 100 °C,
Time 252000 sec
ASTM D395 Method B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0040 ohm-cmCEPS-0002
Shielding Effectiveness >= 100 dB
@Frequency 1e+8 Hz
E Field; CHO-TM-TP08
 >= 100 dB
@Frequency 5.00e+8 Hz
E Field; CHO-TM-TP08
 >= 100 dB
@Frequency 2.00e+9 Hz
Plane Wave; CHO-TM-TP08
 >= 100 dB
@Frequency 1e+10 Hz
Plane Wave; CHO-TM-TP08
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -65.0 °CFlex TR10; ASTM D1329
 
Descriptive Properties
BinderSilicone
FillerAg/Cu
Heat Aging<.01 ohm-cmCEPS-0002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL 1285 Conductive Elastomer
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer

PCHOME120 / 28342

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.