MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics CHO-SEAL 1285 Conductive Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Conductive Elastomer with Improved Corrosion Resistance. This conductive silicone elastomer features significantly improved corrosion resistance in salt spray environments over silver-plated copper-filled silicone, the dominant EMI gasket material for military/aerospace applications since 1962.

Molded and Extruded

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 2.25 g/cc1.75 - 2.25 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 58 - 7258 - 72ASTM D2240
Tensile Strength at Break >= 1.38 MPa>= 200 psiASTM D412
Elongation at Break 100 - 300 %100 - 300 %ASTM D412
Tear Strength 5.25 kN/m30.0 pliASTM D624
Compression Set <= 32 %
@Temperature 100 °C,
Time 252000 sec
<= 32 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0080 ohm-cm0.0080 ohm-cmwithout pressure-sensitive material; MIL-DTL-83528
 0.015 ohm-cm0.015 ohm-cmPost Tensile Set; MIL-DTL-83528
Shielding Effectiveness  >= 60 dB
@Frequency 200000 Hz
>= 60 dB
@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
 >= 100 dB
@Frequency 1e+10 Hz
>= 100 dB
@Frequency 1e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 105 dB
@Frequency 2.00e+9 Hz
>= 105 dB
@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 110 dB
@Frequency 5.00e+8 Hz
>= 110 dB
@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 >= 115 dB
@Frequency 1e+8 Hz
>= 115 dB
@Frequency 1e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.20 W/m-K
@Pressure 2.07 MPa
15.3 BTU-in/hr-ft²-°F
@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °FFlex TR10; ASTM D1329
 
Descriptive Properties
BinderSilicone
EMP Survivability>0.9 kA / in
FillerAg/Al
GradeMilitary-Aerospace/B
Heat Aging<0.01 ohm-cmMIL-DTL-83528 Para.4.6.15
Type BMIL-DTL-83528
Vibration Resistance, After<0.008 ohm-cmMIL-DTL-83528 Para.4.6.13
Vibration Resistance, During<0.012 ohm-cmMIL-DTL-83528 Para.4.6.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
P & P Technology EC-H Silver Copper Loaded Fluorosilicone
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
P & P Technology EC-H Silver Copper Loaded Silicone

PCHOME125 / 28347

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.