MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology EC-H Silver Copper Loaded Fluorosilicone
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer excellent physical and electrical properties over an effective temperature range of –55°C to +160°C. Fluorosilicone offers excellent performance over a wide temperature range with good resistance to chemicals, mineral based oils/greases and weathering.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.60 - 3.80 g/cc3.60 - 3.80 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.50 MPa218 psiASTM D412
Elongation at Break >= 110 %>= 110 %ASTM D412
Compression Set <= 30 %
@Temperature 100 °C,
Time 259000 sec
<= 30 %
@Temperature 212 °F,
Time 72.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0050 ohm-cm<= 0.0050 ohm-cmMil-G-83528
Shielding Effectiveness  75 dB
@Frequency 200000 Hz
75 dB
@Frequency 200000 Hz
Mil-G-83528/Mil std 285
 100 dB
@Frequency 1e+8 Hz
100 dB
@Frequency 1e+8 Hz
Mil-G-83528/Mil std 285
 101 dB
@Frequency 2.00e+9 Hz
101 dB
@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
 105 dB
@Frequency 5.00e+8 Hz
105 dB
@Frequency 5.00e+8 Hz
Mil-G-83528/Mil std 285
 110 dB
@Frequency 1e+10 Hz
110 dB
@Frequency 1e+10 Hz
Mil-G-83528/Mil std 285
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer
Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer
P & P Technology EC-H Silver Copper Loaded Silicone
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive

PPPTEC028 / 133492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.