MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest shielding effectiveness of any conductive elastomer material, in addition to offering excellent moisture sealing for all enclosure joints and seam

Typical Applications: The MIL-DTL-83528 certified compounds meet the demanding requirements of many military and aerospace systems, and as gaskets for waveguides and connectors. In addition, CONSIL-C can also be used for EMP and TEMPEST application

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.045 - 3.955 g/cc3.045 - 3.955 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 9278 - 92ASTM D2240
Tensile Strength >= 2.76 MPa>= 400 psiASTM D412
Elongation at Break 100 - 300 %100 - 300 %ASTM D412
Tear Strength 7.01 kN/m40.0 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0050 ohm-cm<= 0.0050 ohm-cm
Shielding Effectiveness  75 dB
@Frequency 100000 Hz
75 dB
@Frequency 100000 Hz
H-Field
 110 dB
@Frequency 1e+10 Hz
110 dB
@Frequency 1e+10 Hz
Plane Wave
 115 dB
@Frequency 1e+9 Hz
115 dB
@Frequency 1e+9 Hz
Plane Wave
 >= 120 dB
@Frequency 1e+7 Hz
>= 120 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -45.0 °C-49.0 °F
 
Descriptive Properties
BinderSilicone
ColorGray
FillerSilver Plated Copper Particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer
P & P Technology EC-H Silver Copper Loaded Fluorosilicone
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer
P & P Technology EC-H Silver Copper Loaded Silicone
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer

PCHOME380 / 131090

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.