MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell A-C® 580 EAA copolymer
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Ethylene acrylic acid (EAA) copolymer in a prill form, with an acrylic acid (AA) content of 10%, for use in adhesives to promote adhesion to various substrates. It is also used in aqueous floor polishes to provide drag (raising the coefficient of friction) thereby controlling the final coefficient of friction. Its acid number of 75 aids emulsification. Also used in solvent borne coatings to control rheology and provide metallic flake orientation. Used extensively in automotive basecoats.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/cc
Brookfield Viscosity 650 cP
@Temperature 140 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 75
 
Thermal PropertiesOriginal ValueComments
Dropping Point 95.0 °CMettler
 
Descriptive Properties
Hardness4 dmmASTM D5
Product FormPastille

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell A-C® 540A EAA copolymer
Honeywell A-C® 5120 EAA copolymer
Honeywell A-C® 5180 EAA copolymer
Honeywell AClyn® 201 EAA copolymer
Honeywell AClyn® 201A EAA copolymer

PHONWL038 / 179583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.