MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell A-C® 5180 EAA copolymer
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Ethylene acrylic acid (EAA) copolymer in a tacky solid form, with an acrylic acid (AA) content of 20%, for use in adhesives to promote adhesion to various substrates. Its acid number of 180 greatly aids emulsification and it can even be dispersed in water. Also used in solvent borne coatings to control rheology.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³
Brookfield Viscosity 625 cP
@Temperature 140 °C
625 cP
@Temperature 284 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 200200
 
Thermal PropertiesMetricEnglishComments
Dropping Point 76.0 °C169 °FMettler
 
Descriptive Properties
Product FormTacky solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell A-C® 5120 EAA copolymer
Honeywell AClyn® 201 EAA copolymer
Honeywell AClyn® 246 EAA copolymer
ExxonMobil Exxtra™ Adhere EAA38015 Ethylene Acrylic Acid Copolymer Resin
Honeywell A-C® 580 EAA copolymer

PHONWL068 / 179613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.