MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucobit Lucocell® FG3000 Cellulose Asphalt Additive
Categories: Polymer; Thermoplastic; Cellulosic

Material Notes: Lucocell® FG3000 micro grains – cellulose additives for SMA –Stone Mastic Asphalt or Split Mastic Asphalt, which is used as finish for all road types. Due to their 3D structure, cellulose fibers maintain a comparatively high viscosity of bitumen, thus preventing its seepage and formation of asphalt mix segregation at high temperatures during storage, transport and SMA placing. At the same time they enable creation of a thicker bitumen layer around each rock particle, thus preventing oxidation, moisture penetration and lifting or cracking of the aggregate.

Because of the nature of the product cellulose fibers may not be exposed to water and mix temperatures higher than 200°C.

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.450 g/cc
 
Descriptive Properties
Average Fiber Diameter, µm45
Average Fiber Length, µm1100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
FKuR Kunststoff Biograde® C 5509 CL Cellulose Acetate
Rotuba H Cellulose Acetate
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp

PLUCO911 / 150977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.