Description: BR® 57 is a high temperature condensation polyimide primer intended for use with FM® 57 film adhesive and BR® 57-2 paste adhesive. The primer contains no metallic filler. It may be easily spray applied or roller coated.Information provided by Cytec, subsequently acquired by Solvay. |