MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Sorona® FG3301 NC010 PTT  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polytrimethylene Terephthalate (PTT)

Material Notes: Unreinforced, Renewably Sourced, Polytrimethylene Terephthalate Developed for Food Contact Applications

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Melt Density 1.12 g/cc
@Temperature >=228 °C
Linear Mold Shrinkage, Flow 0.013 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPaISO 527-1/-2
Elongation at Break 15 %ISO 527-1/-2
Elongation at Yield 5.5 %ISO 527-1/-2
Tensile Modulus 2400 MPaISO 527-1/-2
Flexural Modulus 2400 MPaISO 178
Poissons Ratio 0.38ISO 527-1/-2
Izod Impact, Unnotched (ISO) 4.50 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 575 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.10 J/g-°C
@Temperature >=228 °C
Melt
Thermal Conductivity 0.200 W/m-K
@Temperature >=228 °C
Melt
Melting Point 228 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °CInjection
 260 °CInjection Optimum
Mold Temperature 80.0 - 110 °CInjection
 100 °CInjection Optimum
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.020 %Injection
 
Descriptive Properties
Back pressureAs low as possibleInjection
Delivery formPellets
Drying RecommendedyesInjection
Part Marking Code>PTT<ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPTTISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Sorona® 2045G BK346A PTT-GF45
DuPont Mobility and Materials Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
DuPont Mobility and Materials Sorona® 3015G BK001 PTT-GF45
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized

PZDSX5290 / 197930

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.