MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polytrimethylene Terephthalate (PTT)

Material Notes: Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance

Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded

Information provided by DuPont.

Key Words: PTT-I
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
 1.23 g/cc0.0444 lb/in³ISO 1183
Water Absorption 0.34 %
@Thickness 2.00 mm
0.34 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.110 %
@Thickness 2.00 mm
0.110 %
@Thickness 0.0787 in
Sim. to ISO 62
Water Absorption at Saturation 0.080 %0.080 %Immersion 24h; ASTM D570
Viscosity  70540 cP
@Shear Rate 5000 1/s,
Temperature 270 °C
70540 cP
@Shear Rate 5000 1/s,
Temperature 518 °F
ISO 11403-1 -2
 75970 cP
@Shear Rate 5000 1/s,
Temperature 260 °C
75970 cP
@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
 82100 cP
@Shear Rate 5000 1/s,
Temperature 250 °C
82100 cP
@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
 277400 cP
@Shear Rate 500 1/s,
Temperature 270 °C
277400 cP
@Shear Rate 500 1/s,
Temperature 518 °F
ISO 11403-1 -2
 312300 cP
@Shear Rate 500 1/s,
Temperature 260 °C
312300 cP
@Shear Rate 500 1/s,
Temperature 500 °F
ISO 11403-1 -2
 351600 cP
@Shear Rate 500 1/s,
Temperature 250 °C
351600 cP
@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inISO 294-4 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psiISO 527-1/-2
Elongation at Break 15 %15 %Nominal; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %ISO 527-1/-2
Tensile Modulus 1.60 GPa232 ksiISO 527-1/-2
Flexural Modulus 1.60 GPa232 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 2.20 J/cm²10.5 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohm6.00e+14 ohmIEC 60093
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength 32.0 kV/mm813 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.0205
@Frequency 1e+6 Hz
0.0205
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 138 µm/m-°C76.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 138 µm/m-°C76.7 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 2.10 J/g-°C0.502 BTU/lb-°F
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°Fof melt
Melting Point 229 °C444 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C127 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PTT-I<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPTT-I

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Sorona® FG3301 NC010 PTT
DuPont Mobility and Materials Sorona® 3015G BK001 PTT-GF45
Overview of materials for Polytrimethylene Terephthalate (PTT)
Polyglycolic Acid (PGA)
Polydioxanone

PZDSY5304 / 161131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.