MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors and housings for electronic units under the hood.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 - 0.900 g/cc
Density 1.51 g/ccISO 1183
Water Absorption 0.40 %ISO 62
Moisture Absorption at Equilibrium 0.20 %ISO 62
Viscosity Test 108 cm³/gISO 307
Linear Mold Shrinkage, Flow 0.0045 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527-1/-2
Elongation at Break 3.3 %ISO 527-1/-2
Tensile Modulus 8700 MPaISO 527-1/-2
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °CISO 11357-1/-2
Maximum Service Temperature, Air 210 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Decomposition Temperature >= 290 °C
Ignition Temperature 350 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 250 °CFeeding zone
Zone 2 255 °CCompression
Zone 3 260 °CMetering-zone
Zone 4 260 °CNozzle
Melt Temperature 260 °COptimal
 250 - 275 °CInjection molding/Extrusion
Mold Temperature 60.0 - 100 °CInjection molding
 80.0 °COptimal
Drying Temperature 80.0 - 120 °C
Dry Time 4 hour
 
Descriptive Properties
ColorBK 15116
Commercial StatusEurope
Peripheral Screw Speed<0.25 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT

PBASG0127 / 131760

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.