MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Pearlbond™ 302 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: PEARLBOND™ 302 is a high performance aromatic polyester-based thermoplastic polyurethane (TPU) for use in hot melt adhesives applications (including film & sheet). This is a soft plasticizer-free TPU with excellent low temperature flexibility.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52 - 58ISO 868
Tensile Strength 12.0 - 16.0 MPaISO 527
Elongation at Break 850 - 950 %ISO 527
100% Modulus 1.10 - 1.50 MPa
@Strain 100 %
ISO 527
300% Modulus 1.60 - 2.00 MPa
@Strain 300 %
ISO 527
 
Processing PropertiesOriginal ValueComments
Zone 1 120 - 130 °C
Zone 2 130 - 140 °C
Zone 3 140 - 150 °C
Zone 4 145 - 155 °C
Die Temperature 145 - 155 °C
Screw Speed 20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals SKYTHANE® T870A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Miracll A885 Aliphatic TPU-A Series
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer

PLUBR5038 / 238908

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.