MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.

Benefits of Estane® TPU:

  • Outstanding Abrasion and Wear Resistance
  • Excellent Low Temperature Flexibility
  • Superior Toughness and Durability
  • Ease of Processing and Manufacturing Flexibility
  • Colorability and Paintability with no adhesion promoter
  • Applications:

    • Film & Sheet
    • Fabric coating & melt coating
    • Wire & Cable
    • Hose, Tube & Profile
    • Custom molding
    • Custom compounding
    • Automotive interior/chassis and exterior painted trim

    Specific Notes for this Material: Good hydrocarbon resistance

    Information provided by Noveon, Inc.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 9393ASTM D2240
    Hardness, Shore D 4545ASTM D224
    Tensile Strength, Ultimate 31.7 MPa4600 psiASTM D412/D638
    Elongation at Break 450 %450 %ASTM D412/D638
    Flexural Modulus 0.0310 GPa4.50 ksiASTM D790
    Taber Abrasion, mg/1000 Cycles 2.62.6CS-17; ASTM D3389 B
    Compression Set 28 %28 %ASTM D395
    Tensile Set 17 %17 %ASTM D412/D638
     
    Thermal PropertiesMetricEnglishComments
    Vicat Softening Point 107 °C225 °FASTM D1525
    Transformation Temperature -17.2 °C1.00 °Fby DSC

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    LyondellBasell Lupolen 2420H Low Density Polyethylene (LDPE), Film Grade
    Dow LDPE 640I Low Density Polyethylene, Liner Film Grade
    Chase Plastics CP Pryme® APC100 ABS Polycarbonate Alloy
    Covestro DUREFLEX® PT6400 TPU
    Geon® Performance Solutions Vinyl Flexible XV3432 Polyvinyl Chloride, Flexible

    PNOVEON020 / 55286

    Polyurethane

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.