MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crucible Steel CPM® Rex® 20® (HS) High Speed Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wear resistance and greater toughness. CPM Rex 20 was originally designed to replace M42 in any application where cobalt is undesirable. Due to its unique combination of properties, CPM Rex 20 is used in non-cutting applications such as bearings and in plasticizing components such as screw segments, barrels and non-return valves.

The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.17 g/cc0.295 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 262 - 285262 - 285Annealed
Hardness, Rockwell C 65.565.5Hardening Temperature- 1150°C; Tempering Temperature- 550°C
 67.567.5Hardening Temperature- 1205°C; Tempering Temperature- 550°C
Modulus of Elasticity 235 GPa34100 ksi
Flexural Strength 3957 MPa573900 psiHardening Temperature- 1150°C, Tempering Temperature- 550°C
 4005 MPa580900 psiHardening Temperature- 1190°C, Tempering Temperature- 550°C
Charpy Impact 16.0 J11.8 ft-lbHardening Temperature- 1190°C; Tempering Temperature- 550°C
 18.0 J13.3 ft-lbHardening Temperature- 1150°C; Tempering Temperature- 550°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.66 µm/m-°C
@Temperature 20.0 - 94.0 °C
5.922 µin/in-°F
@Temperature 68.0 - 201 °F
 11.18 µm/m-°C
@Temperature 20.0 - 205 °C
6.211 µin/in-°F
@Temperature 68.0 - 401 °F
 12.24 µm/m-°C
@Temperature 20.0 - 540 °C
6.800 µin/in-°F
@Temperature 68.0 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.3 %1.3 %
Chromium, Cr 3.75 %3.75 %
Iron, Fe 75.92 %75.92 %As Remainder
Molybdenum, Mo 10.5 %10.5 %
Sulfur, S 0.060 - 0.22 %0.060 - 0.22 %
Tungsten, W 6.25 %6.25 %
Vanadium, V 2.0 %2.0 %
 
Descriptive Properties
Grindability; Metal Removed/Wheel Worn3.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS)
Crucible Steel CPM® Rex® 45® (HS) High Speed Steel
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel

NCRUC007 / 16000

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.