MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayfill® 53IF40 U Polyurethane Structural Foam RIM
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: This is a semi-rigid polyurethane foam system composed of Bayfill 53IF40 U polyol blend and Desmodur® 58IF07 M polyisocyanate.

Properties / Applications: This is a semi-rigid polyurethane foam system composed of Bayfill 53IF40 U polyol blend and Desmodur® 58IF07 M polyisocyanate. It is used in the production of soft-touch panels, such as automotive instrument panels. The foam system is supplied as two liquid components. Component A, Desmodur 58IF07 M, is a polymeric diphenylmethane diisocyanate product. Component B , Bayfill 53IF40 U, is a formulated polyether polyol blend. As with any product, use of Bayfill 53IF40 U system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.138 g/cc0.138 g/ccASTM D3574
 1.03 g/cc1.03 g/ccPolyol (Component B)
 1.24 g/cc1.24 g/ccIsocyanate (Component A)
Viscosity 50 - 60 cP50 - 60 cPIsocyanate (Component A)
 1500 cP1500 cPPolyol (Component B)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.310 MPa45.0 psiASTM D3574
Elongation at Break 70 %70 %ASTM D3574
Compressive Strength 0.0750 MPa
@Strain 50 %
10.9 psi
@Strain 50 %
ASTM D3574
Compression Set 10 %10 %50% compression; ASTM D3574
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 199 °C>= 390 °FPMCC, Polyol (Component B)
 >= 200 °C>= 392 °FPMCC, Isocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 40.0 °C104 °Flid
 42.0 °C108 °Fcavity
 
Descriptive Properties
AppearanceBlack liquidPolyol (Component B)
 Dark brown liquidIsocyanate (Component A)
Content>32%NCO, Isocyanate (Component A)
Hydroxyl number[mg KOH/g], Polyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayfill® EA 2001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
Elliott Company ELFOAM® P200 Polyisocyanurate Foam
BCC Products MB 1100 Polyurethane Foam Modeling Board
Covestro Baydur® 40 Polyurethane
Covestro Bayfill® 310 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System

PCOVEST0106 / 201889

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.