(Viewing data as-entered.
Click here
to return)
Teknor Apex Chemlon® A25 Nylon 66, Conditioned
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced
Material Notes:
Notes:
A25 is a standard, unfilled injection molding grade of nylon 66.
Availability:
Europe
Form:
Pellets
Processing Method:
Injection Molding
Information provided by Teknor Apex
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.14
g/cc
ISO 1183
Moisture Absorption at Equilibrium
1.2 %
50% RH; ISO 62
Linear Mold Shrinkage
0.011
-
0.017
in/in
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
8700
psi
ISO 527-2
Tensile Modulus
232000
psi
ISO 527-2
Flexural Strength
5080
psi
ISO 178
Flexural Modulus
145000
psi
ISO 178
Charpy Impact Unnotched
NB
ISO 179
Charpy Impact, Notched
NB
ISO 179
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+11
ohm
IEC 60093
Dielectric Constant
4.3
IEC 60250
Dielectric Strength
300
V/mil
@Thickness 3.00 mm
IEC 60243-1
Dissipation Factor
0.080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
>=
600
V
IEC 60112
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
401
°F
Unannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi)
176
°F
Unannealed; ISO 72-2/A
Processing Properties
Original Value
Comments
Rear Barrel Temperature
518
-
554
°F
Middle Barrel Temperature
518
-
554
°F
Front Barrel Temperature
518
-
554
°F
Melt Temperature
>=
572
°F
Mold Temperature
140
-
176
°F
Drying Temperature
176
-
212
°F
Dry Time
2.00
hour
Screw Speed
50
-
200
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PTEKNQ0539 / 237030
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.