System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Teknor Apex Chemlon® A25 Nylon 66, Conditioned
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced
Material Notes:
Notes:
A25 is a standard, unfilled injection molding grade of nylon 66.
Availability:
Europe
Form:
Pellets
Processing Method:
Injection Molding
Information provided by Teknor Apex
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.14
g/cc
0.0412
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
1.2 %
1.2 %
50% RH; ISO 62
Linear Mold Shrinkage
0.011
-
0.017
cm/cm
0.011
-
0.017
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
60.0
MPa
8700
psi
ISO 527-2
Tensile Modulus
1.60
GPa
232
ksi
ISO 527-2
Flexural Strength
35.0
MPa
5080
psi
ISO 178
Flexural Modulus
1.00
GPa
145
ksi
ISO 178
Charpy Impact Unnotched
NB
NB
ISO 179
Charpy Impact, Notched
NB
NB
ISO 179
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+11
ohm
1.00e+11
ohm
IEC 60093
Dielectric Constant
4.3
4.3
IEC 60250
Dielectric Strength
11.8
kV/mm
@Thickness 3.00 mm
300
kV/in
@Thickness 0.118 in
IEC 60243-1
Dissipation Factor
0.080
@Frequency 1e+6 Hz
0.080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
>=
600
V
>=
600
V
IEC 60112
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
205
°C
401
°F
Unannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi)
80.0
°C
176
°F
Unannealed; ISO 72-2/A
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
270
-
290
°C
518
-
554
°F
Middle Barrel Temperature
270
-
290
°C
518
-
554
°F
Front Barrel Temperature
270
-
290
°C
518
-
554
°F
Melt Temperature
>=
300
°C
>=
572
°F
Mold Temperature
60.0
-
80.0
°C
140
-
176
°F
Drying Temperature
80.0
-
100
°C
176
-
212
°F
Dry Time
2.00
hour
2.00
hour
Screw Speed
50
-
200
rpm
50
-
200
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PTEKNQ0539 / 237030
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.