MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP545 Carbon Fiber  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gauge systems, high performance gears and bearings, and pump and compressor vanes.

Thickness Tested: 0.062", 0.125" and 0.500"

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 - 1.70 g/cc
@Thickness 1.57 mm
ASTM D792
Moisture Absorption at Equilibrium 0.10 %
@Thickness 1.57 mm
ASTM D229
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95 - 115
@Thickness 1.57 mm
ASTM D785
Tensile Strength, Yield 71000 psi
@Thickness 1.57 mm
CW; ASTM D638
 72000 psi
@Thickness 1.57 mm
LW; ASTM D638
Modulus of Elasticity 5300 ksi
@Thickness 1.57 mm
CW; ASTM D229
 6000 ksi
@Thickness 1.57 mm
LW; ASTM D229
Flexural Strength 98000 psi
@Thickness 1.57 mm
CW; ASTM D790
 98500 psi
@Thickness 1.57 mm
LW; ASTM D790
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 8.00 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 177 °C
Glass Transition Temp, Tg 125 °CTg
Flammability, UL94 HB
@Thickness 1.57 mm
 
Descriptive Properties
Bond Strength1200 lb0.5", ASTM D229
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Norplex-Micarta NP555 Carbon Fiber
DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors

PNORPN565 / 48150

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.