MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP555 Carbon Fiber  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Phenolic

Material Notes: Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane material for large, high performance compressors.

Thickness Tested: 0.062", 0.125" and 0.500"

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 - 1.60 g/cc
@Thickness 1.57 mm
1.50 - 1.60 g/cc
@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 0.10 %
@Thickness 1.57 mm
0.10 %
@Thickness 0.0620 in
ASTM D229
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 95 - 115
@Thickness 1.57 mm
95 - 115
@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield  379 MPa
@Thickness 1.57 mm
55000 psi
@Thickness 0.0620 in
CW; ASTM D638
 552 MPa
@Thickness 1.57 mm
80000 psi
@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity  8.27 GPa
@Thickness 1.57 mm
1200 ksi
@Thickness 0.0620 in
CW; ASTM D229
 8.96 GPa
@Thickness 1.57 mm
1300 ksi
@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength  323 MPa
@Thickness 1.57 mm
46800 psi
@Thickness 0.0620 in
CW; ASTM D790
 381 MPa
@Thickness 1.57 mm
55200 psi
@Thickness 0.0620 in
LW; ASTM D790
Izod Impact, Unnotched  19.8 J/cm
@Thickness 12.7 mm
37.0 ft-lb/in
@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
 21.4 J/cm
@Thickness 12.7 mm
40.0 ft-lb/in
@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
3.33 µin/in-°F
@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 11.0 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
6.11 µin/in-°F
@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 230 °C446 °F
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
 
Descriptive Properties
Bond Strength600 lb0.5", ASTM D229
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta NP185 Carbon Fiber
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Solvay LTM® 26EL Epoxy with 34-700 Unidirectional Carbon Laminate Prepreg
Norplex-Micarta NP545 Carbon Fiber

PNORPN566 / 48151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.