MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Elastosil® R 512/70 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: ELASTOSIL® R 512/70 is a peroxide crosslinking HCR silicone for the manufacture of silicone-insulated safety cables that maintain circuit integrity in case of fire.

Properties: The color of the rubber base is white. Therefore, preliminary tests are required to match the RAL color of the masterbatches used in paste or pellet form in the compound (pastel colors).

Special features:

  • good mechanical and electrical properties
  • good rheological properties
  • good heat stability
  • in case of fire formation of a ceramic-like layer with high insulation resistance and good mechanical stability without formation of corrosive or toxic gases
  • in case of fire low smoke density
  • remains functional above 950°C in case of fire
Application: For flame resistant cable constructions (safety cables). Cables made of ELASTOSIL® R 512/70 have successfully passed standards, like NFC 32070 CR1, DIN 4102 part 12, UL 2196, EN 50200, IEC 60331-11, etc.

Ratio: ELASTOSIL® R 512/70-1 : ELASTOSIL® R 512/70-2

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³2:8; DIN 53479
 1.32 g/cc0.0477 lb/in³3:7; DIN 53479
 1.35 g/cc0.0488 lb/in³DIN 53479
 1.37 g/cc0.0495 lb/in³4:6; DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70702:8; DIN 53505
 70703:7; DIN 53505
 70704:6; DIN 53505
 7575DIN 53505
Tensile Strength at Break 6.00 MPa870 psi4:6; DIN 53504 S1
 7.00 MPa1020 psi3:7; DIN 53504 S1
 8.00 MPa1160 psi2:8; DIN 53504 S1
 8.00 MPa1160 psiDIN 53504 S1
Elongation at Break 300 %300 %3:7; DIN 53504 S1
 300 %300 %4:6; DIN 53504 S1
 320 %320 %2:8; DIN 53504 S1
 380 %380 %DIN 53504 S1
Tear Strength 20.0 kN/m114 pli2:8; ASTM D624 B
 20.0 kN/m114 pli3:7; ASTM D624 B
 20.0 kN/m114 pli4:6; ASTM D624 B
 20.0 kN/m114 pliASTM D624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm2:8; DIN IEC 93
 1.00e+14 ohm-cm1.00e+14 ohm-cm3:7; DIN IEC 93
 1.00e+14 ohm-cm1.00e+14 ohm-cm4:6; DIN IEC 93
 1.00e+14 ohm-cm1.00e+14 ohm-cmDIN IEC 93
Dielectric Constant 2.82.82:8; DIN VDE 0303
 3.03.03:7; DIN VDE 0303
 3.03.04:6; DIN VDE 0303
 3.2
@Frequency 50 Hz
3.2
@Frequency 50 Hz
DIN VDE 0303
Dielectric Strength 16.0 kV/mm406 kV/in4:6; DIN IEC 243-1
 19.0 kV/mm483 kV/in2:8; DIN IEC 243-1
 20.0 kV/mm508 kV/in3:7; DIN IEC 243-1
 25.0 kV/mm635 kV/inDIN IEC 243-1
 
Descriptive Properties
Appearanceopaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3004/70 A/B Liquid Silicone Rubber
Seals Eastern 5803 Fluoro-silicone
Rogers Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate
NuSil MED-4565 One-Part Standard High Consistency Elastomer - Unrestricted Medical Use

PWACK9220 / 204749

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.