MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oceanchem Group Brominated Epoxy Oligomers-3 (BEP-3)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Epoxy

Material Notes: Molecular Formula: (C36H32Br8O6)n

Cas No.: 68928-70-1

Application: BEP-3 is a high molecular weight brominated epoxy polymeric flame retardant designed for a broad range of thermoplastic applications. BEP-3 is recommended for thermoplastic polyesters (PBT, PET), thermoplastic polyurethanes (TPU), alloys (PC/ABS), styrenics (ABS, HIPS) and others. The specially selected molecular weight and the chemical structure of BEP-3 offers high thermal stability and thermal ageing, excellent processability, non-blooming, and good UV stability. BEP-3 offers a similar combination of properties to that of BEP-3 for those applications where higher melf flow (MFI) values are required.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
 
Thermal PropertiesMetricEnglishComments
Softening Point 145 - 155 °C293 - 311 °F
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 53.0 %53.0 %
 
Descriptive Properties
AppearanceLight Yellow Granules
CAS Number68928-70-1
Molecular Formula(C36H32Br8O6)n
Weight Loss (%)10353°C
 2339°C
 5347°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 185 Urethane Thermoplastic Elastomer
Covestro DUREFLEX® PT6400 TPU
Covestro Desmopan® 3378A TPU
Covestro Desmopan® 3360A DPS 061 TPU
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU

POCEAN29 / 104233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.