MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Texin® 185 Urethane Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Key Features:
  • Unfilled

Suitable processing methods:

  • Injection molding
  • Film extrusion
  • Profile extrusion
  • Sheet extrusion
  • Coating

Information provided by Bayer Polymers.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress at Strain 6.00 MPa
@Strain 50 %
870 psi
@Strain 50 %
Elongation at Break >= 50 %>= 50 %
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 88.0 °C190 °F50°C/h 50N
Glass Transition Temp, Tg -30.0 °C-22.0 °F10°C/min
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 °C383 °FInjection Molding
Mold Temperature 30.0 °C86.0 °FInjection Molding
Injection Pressure 45.0 MPa6530 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
Covestro Texin® 945U Urethane Thermoplastic Elastomer
Covestro Texin® 390 Urethane Thermoplastic Elastomer
Covestro Texin® 950 Urethane Thermoplastic Elastomer
Covestro Texin® DP 7-1158 Urethane Thermoplastic Elastomer

PB10315 / 26353

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.