MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: M3766 is an isostatic form of polypropylene made via TOTAL proprietary technology.

Recommended Applications. M3766 is recommended for melt spun and spun bound fiber applications. However, due to its unique and interesting properties, other applications may exist.

Processing. M3766 is a narrower molecular weight distribution product that conventional polypropylene.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 23 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Elongation at Yield 185 %ASTM D3218
Tenacity 2.50 g/denierASTM D3218
 
Thermal PropertiesOriginal ValueComments
Melting Point 151 °CDSC
 
Descriptive Properties
Xylene Solubles0.7 to 1.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 7069 Polypropylene, Homopolymer
Total PPH 4060 Polypropylene, Homopolymer
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
Total PPH 3270 Polypropylene Homopolymer, High Crystallinity, Low Melt Flow Film Grade

PTOTAL806 / 130531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.