MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPH 4060 Polypropylene, Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA Polypropylene PPH 4060 is homopolymer.

Application

ATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is also a general purpose injection grade for molding technical items.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ISO 2039-2
Tensile Strength, Yield 33.0 MPa4790 psiISO 527-2
Elongation at Yield 10 %10 %ISO 527-2
Tensile Modulus 1.45 GPa210 ksiISO 527-2
Flexural Modulus 1.35 GPa196 ksiISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 179
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °F120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F120°C per hour; ISO 75-2
Vicat Softening Point 85.0 °C185 °F50N-50°C per hour; ISO 306
 150 °C302 °F10N-50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 9021 POM, Unfilled
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced
Celanese Hostaform® C 13021 POM, Unfilled
Overview of materials for Polypropylene, Molded
Celanese Hostaform® C 9021 TF POM, Tribological

PFINAA119 / 38555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.