MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: EPOCYL™ NC E128-04 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed for solvent based formulations to enhance the electrical conductivity of final epoxy formulations. Special features include easy integration and great flexibility in processing. Dilution factor has to be calculated accordingly to the desired level of conductivity.

Applications

  • Electrostatic discharge (ESD) coatings, linings (tanks, rollers, ...) and composites
  • Conductive primers
  • Resistive inks
  • Adhesives

Benefits

  • Limited impact on base resin mechanical and thermo-mechanical properties
  • Ease of formulation
  • Other information available upon request to Nanocyl

Curing agents EPOCYL™ NCE128-04 based formulations can be cured or cross-linked with different types of curing agents which could be decided accordingly to the desired processing conditions and the properties of the final composite like any conventional Bis-A based formulations.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 - 1.20 g/cc1.15 - 1.20 g/cc
Viscosity 25000 - 45000 cP
@Temperature 25.0 °C
25000 - 45000 cP
@Temperature 77.0 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3000 ohm-cm3000 ohm-cm53 parts per 100 of NC E128-04 in the final compound
 20000 ohm-cm20000 ohm-cm26 parts per 100 of NC E128-04 in the final compound
 70000 ohm-cm70000 ohm-cm13 parts per 100 of NC E128-04 in the final compound
 
Descriptive Properties
AspectPaste, black (Master Batch)
Epoxy Equivalent196.1 - 203.52 g/eq
Epoxy Value4.91 - 5.1 eq/kg
Storage Temperature5°C - 40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6
Overview of materials for Epoxy/Carbon Fiber Composite
NRI Thermo-Wrap™ CF Carbon Fiber Composite
NRI Thermo-Wrap™
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System

PNANOCY991 / 108947

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.