MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Cellular 87018 PVC, Rigid  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Physical Properties were measured on flat cellular profiles with a 0.72 specific gravity natural compound. The Cell Classification was determined using the notched Izod test with injection molded samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.599 - 0.748 g/ccCellular; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73
@Time 15.0 sec
ASTM D2240
Tensile Strength, Yield 14.8 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 1060 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 30.2 MPaASTM D790
Flexural Modulus 1360 MPaASTM D790
Izod Impact, Notched 32.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Across Flow, Compression Molded; ASTM D256A
 48.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 96.1 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Flow, Compression Molded; ASTM D256A
Dart Drop Total Energy 8.90 J/cm
@Temperature 23.0 °C
Procedure B, C.125 Dart; ASTM D4226
 8.90 J/cm
@Temperature 23.0 °C
Procedure A, C.125 Dart; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 V-0UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 193 °C
 
Descriptive Properties
FormsCellular
 Pellets
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Molded
European Alder Wood
Overview of materials for PVC, Foam Grade
Vycom CELTEC® Expanded Rigid foam PVC board
Geon® Performance Solutions Vinyl Cellular E2519 Polyvinyl Chloride, Rigid

PH1PN8219 / 102055

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.