MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Cellular E2519 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccCellular; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Tensile Strength, Yield 55.1 MPa7990 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.92 GPa424 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 94.5 MPa13700 psiASTM D790
Flexural Modulus 3.02 GPa438 ksiASTM D790
Izod Impact, Notched 0.450 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.843 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy  53.8 J/cm
@Temperature 23.0 °C
0.101 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 53.8 J/cm
@Temperature 23.0 °C
0.101 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C37.2 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi)  79.4 °C
@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
175 °F
@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
 79.4 °C
@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
175 °F
@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  75.6 °C
@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
168 °F
@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
 76.2 °C
@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
169 °F
@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
 
Descriptive Properties
FormsCellular, Free Blow
 Cellular, Inward Foam
 Powder
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConsumer Applications
 Cosmetics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 8150 Rigid PVC, Extrusion & Molding
Axiall 1601 Clear 7002 Flexible PVC
Colorite Polymers 2007 Rigid PVC
Colorite Polymers 2019F Rigid PVC
European Alder Wood

PH0POL1389 / 145958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.