Levagard® DMPP is a halogen free flame retardant with a very high phosphorus content and low viscosity. The flame retardant effect is excellent. Chemical composition: Dimethyl propane phosphonate (DMPP) CAS-Reg.- No. 18755-43-6 Applications: Levagard® DMPP is suitable for PIR / PUR rigid foams and thermosets. Information provided by Lanxess. |