MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess Levagard® DMPP Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Levagard® DMPP is a halogen free flame retardant with a very high phosphorus content and low viscosity. The flame retardant effect is excellent.

Chemical composition: Dimethyl propane phosphonate (DMPP)

CAS-Reg.- No. 18755-43-6

Applications: Levagard® DMPP is suitable for PIR / PUR rigid foams and thermosets.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.072 g/cc0.03873 lb/in³
Water Absorption <= 0.10 %<= 0.10 %
Viscosity 2.5 cP2.5 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.50<= 0.50[mg KOH/g]
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4197 - 1.42271.4197 - 1.4227
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month9.00 Month
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 20.3 %20.3 %
 
Descriptive Properties
Appearanceclear, colorless liquid
Color<20Hazen
Content>98%DMPP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8676 / 209069

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.