MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Eccobond® 59C One-Component Silver Filled Electrically Conductive Silicone Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Emerson & Cuming 59C Eccobond® One-Component Silver Filled Electrically Conductive Silicone Adhesive
One component, solvent containing, silver filled, electrically conductive, silicone pressure sensitive adhesive. High flexibility. High tack. Bonds formed can be repeatedly opened and sealed. Bonding Type: Silicone

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 300 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0010 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.300 hour
@Temperature 25.0 °C
 
Descriptive Properties
ColorSilver
ViscosityThixotropic (Mixed, 25°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
P & P Technology Silver/Aluminum Conductive Adhesive
Overview of materials for Epoxy, Electrically Conductive
Master Bond FL901S One Component, Silver Filled Epoxy
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide
Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy

PEMERS54 / 35746

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.