MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of flow characteristics. This epoxy has a 90 minute worklife and is a 1:1 mix ratio. Ideal for bulk application through meter mix dispensing equipment and the manufacture of large panel products.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 17200 cPBase, RVF #7 sp @ 20 rpm
 68200 cPAccelerator, RVF #7 sp @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60 - 65
Shear Strength 480 psiOverlap, Polycarbonate-IPA/abrade/IPA, Adhesive Failure
 2000 psiOverlap, FRP(Green)-IPA/abrade/IPA, Cohesive Failure
 2700 psiOverlap, FRP(Red)-IPA/abrade/IPA, Substrate Failure
 3200 psiOverlap, CRS-MEK/Abrade/MEK, Cohesive/Adhesive Failure
 3400 psiOverlap, Galvanized Steel-MEK/Abrade/MEK, Cohesive/Adhesive Failure
 3600 psiOverlap, Al-MEK/Abrade/MEK, Cohesive Failure
 3700 psiOverlap, Stainless Steel-MEK/Abrade/MEK, Cohesive/Adhesive Failure
 4100 psiAluminum, etched, Overlap, 30 day Gasoline soak, Cohesive Failure
 4500 psiAluminum, etched, Overlap, 30 day 65°C/80% RH, Cohesive Failure
 4600 psiAluminum, etched, Overlap, 30 day water soak, Cohesive Failure
 4700 psiAluminum, etched, Overlap, 30 day IPA soak, Cohesive Failure
 4800 psiAluminum, etched, Overlap, Control, Cohesive Failure
 3400 psi
@Temperature -55.0 °C
Aluminum, etched, Overlap, Cohesive Failure
 4500 psi
@Temperature 23.0 °C
Aluminum, etched, Overlap, Cohesive Failure
 400 psi
@Temperature 121 °C,
Time 900 sec
Aluminum, etched, Overlap, Adhesive Failure
 900 psi
@Temperature 82.0 °C,
Time 14400 sec
Aluminum, etched, Overlap, Adhesive Failure
 1200 psi
@Temperature 82.0 °C,
Time 900 sec
Aluminum, etched, Overlap, Adhesive Failure
Peel Strength 56.5 pliAl to Al, Honeycomb Climbing Drum Peel; ASTM D1781
 3.60 pli
@Temperature -55.0 °C
Aluminum, etched, Bell Peel, Cohesive Failure; ASTM D3167
 13.3 pli
@Temperature 23.0 °C
Aluminum, etched, Bell Peel, Adhesive Failure; ASTM D3167
 15.9 pli
@Temperature 82.0 °C,
Time 14400 sec
Aluminum, etched, Bell Peel, Adhesive Failure; ASTM D3167
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 hourTime to Handling Strength
 168 hourFull Cure
 
Descriptive Properties
AppearanceDark GrayAccelerator
 Gray
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding
Master Bond EP36 High Temperature Resistant, Toughened Epoxy System
Master Bond EP21TDC Toughened, Shock Resistant Two Component Epoxy System
Master Bond EP125 High Temperature Resistant, Toughened Epoxy System

PMM34778 / 169525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.