MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applications where long term exposure to temperatures from -78°to +450°F (-55°to+228°C) is required. It is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly at elevated temperatures with a 100 to 30 mix ratio, by weight, to produce high bonding strengths at both ambient and elevated temperatures which unlike that of many other epoxy adhesives, are relatively insensitive to small changes in the mix ratio or substrate cleaning procedures. Master Bond Polymer Adhesive SUPREME 45HTND can be applied without sagging or dripping on vertical surfaces. It produces durable high strength and tough bonds which are resistant to thermal cycling and chemicals including water, oil and most organic solvents over the wide temperature range of -80°F to more than +450°F. Adhesion to metals, glass, ceramics, wood, vulcanized rubber and many plastics is excellent. The hardened adhesive is an electrical insulator, Color of Part A is gray, part B is clear brown. Master Bond Polymer Adhesive SUPREME 45HTND is widely used in aerospace, electronic, electrical, computer, construction, metal working, appliance, automotive and chemical industries.

Product Advantages:

  • Convenient mixing: product properties relatively unaffected by small changes in mix ratio
  • Surface cleanliness not critical for good bonding in many uses but needed for optimal strength
  • Easy application contact pressure only required for cure, adhesive spreads evenly and smoothly; no drip application feature
  • Convenient cure schedules: long pot life at room temperature and fast elevated temperature cures as required
  • High bonding strength to similar and dissimilar substrates with superior peel strength
  • Superior durability, thermal shock and chemical resistance
  • 100% reactive and does not contain any solvents or diluents
  • Resists ET0 sterilization

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 15.9 MPa>= 2300 psiBond, Al to Al, after 30 days water immersion
 >= 17.2 MPa>= 2500 psiBond, Al to Al
Peel Strength >= 2.10 kN/m>= 12.0 pli
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 180 min
@Temperature 135 - 163 °C
2.00 - 3.00 hour
@Temperature 275 - 325 °F
Pot Life >= 720 min>= 720 min200 gram mass
 >= 720 min>= 720 min1 quart mass
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
 
Descriptive Properties
Mixing Ratio (A to B)100/30by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive
Permabond TA440 Toughened Acrylic Adhesive
Dymax Light Weld® 401 High Clarity Glass Bonding Adhesive
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives

PMASTB359 / 149606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.