MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 200 AR 15 Nylon 6/6 (PA), Aramid Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Aramid Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D 792
Filler Content 15 %Primary Additive
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13000 psiASTM D 638
Elongation at Break 6.0 - 8.0 %ASTM D 638
Tensile Modulus 600 ksiASTM D 638
Flexural Strength 20000 psiASTM D 790
Flexural Modulus 600 ksiASTM D 790
Izod Impact, Notched 0.800 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 10.5 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 - 1.00e+16 ohm-cmASTM D 257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 300 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 530 - 570 °F
Mold Temperature 150 - 225 °F
Drying Temperature 175 °F
Dry Time 4 hour
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
Overview of materials for Nylon 66, Aramid Fiber Filled
Overview of materials for Nylon 612, Aramid Fiber Filled
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
LNP Lubricomp® RA-1004 Polyamide 66, Aramid Fiber Reinforced

PQZWA2924 / 91424

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.