MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Seals Eastern 7042 Fluorocarbon-Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.

Features:

  • Type 1 (Viton A)
  • Chemical and heat resistant

Viton® is a registered trademark of DuPont. Information provided by Seals Eastern.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.83 g/ccASTM D297, 15
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 85ASTM D2240
 95Average; ASTM D2240
 96Dry Heat Aging 392°F; 70 hr; ASTM D865
Tensile Strength >= 1437 psiASTM D412 Method A
 1893 psiAverage; ASTM D412 Method A
 2026 psiDry Heat Aging 392°F; 70 hr; ASTM D865
Tensile Stress at Strain 740 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 850 psi
@Strain 50 %
ASTM D412 Method A
 1105 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 1200 psi
@Strain 100 %
ASTM D412 Method A
 1550 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 63 %ASTM D412 Method A
 97 %Dry Heat Aging 392°F; 70 hr; ASTM D865
 101 %Average; ASTM D412 Method A
Compression Set 18 %
@Temperature 200 °C,
Time 79200 sec
ASTM D395, Test B
 32 %
@Temperature 200 °C,
Time 252000 sec
ASTM D395, Test B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -17.0 °FRetraction Temperature, TR10; ASTM D1329
Brittleness Temperature -30.0 °FASTM D746
Glass Transition Temp, Tg -4.00 °FASTM D1329
 
Processing PropertiesOriginal ValueComments
Shelf Life 120 Month
 
Descriptive Properties
Strain Energy/ Unit Volume at 20% Elongation (psi)87ASTM D412 Method A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary PVC 2235RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic
Precision Polymer Engineering E90Q Ethylene Propylene Rubber
AlphaGary PVC 2212-100 CLEAR 0003 Polyvinyl Chloride Thermoplastic
Chemours Viton® A-700 with 65 phr N990 Carbon Black
Chemours Viton® A-401C with 60 MT Black Fluoroelastomer Compound

PSEAL904 / 139297

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.