MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.

Nylon 6 with 50% long glass fiber reinforcement

Information provided by PlastiComp, Inc.

Key Words: Complet® Long Fiber LGF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.56 g/ccASTM D-792
Filler Content 50 %Long Glass Fiber
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 228 MPaASTM D-638
Elongation at Break 1.0 - 2.0 %ASTM D-638
Tensile Modulus 16207 MPaASTM D-638
Flexural Strength 352 MPaASTM D-790
Flexural Modulus 15172 MPaASTM D-790
Izod Impact, Notched 347 J/mASTM D-256
Izod Impact, Unnotched 1495 J/mASTM D-4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 216 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 530 °F
Middle Barrel Temperature 510 - 540 °F
Front Barrel Temperature 520 - 550 °F
Nozzle Temperature 520 - 550 °F
Melt Temperature 520 - 550 °F
Mold Temperature 200 °F
Injection Velocity 2.00 - 3.00 in/sec
Drying Temperature 85.0 °C
@Time 14400 sec
Moisture Content <= 0.18 %
Back Pressure 25.0 - 50.0 psi
Cushion 0.250 in
Screw Speed 30 - 50 rpm
 
Descriptive Properties
Injection PressureMedium to maximum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnForce™ LFT NN-30 LCF/000 Natural Nylon 66 with 30% Long Carbon Fiber
Overview of materials for Nylon 6, Unreinforced
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified

PPLASTI914 / 159325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.