Description: AKROMID B3 GF 15 1 black (4670) is a 15% glass fiber reinforced and heat stabilized polyamide-blend with a reduced density compared to standard PA GF 15. Applications are mainly technical components in the automotive and electronic industry, where a weight and cost reduction is required. Additive: Heat Stabilizer Features: - Low Density
- Heat Stabilized
Uses:- Automotive Application
- Electrical/Electronic Applications
- Engineering Parts
Information provided by Akro-Plastic GmbH |