MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.3 %2.3 %50% RH
 2.3 - 2.9 %2.3 - 2.9 %23°C; 50% RH; ISO 62
 7.7 %7.7 %Saturation
Water Absorption at Saturation 7.7 - 8.3 %7.7 - 8.3 %ISO 62
Viscosity Measurement 140140ISO 307
Linear Mold Shrinkage 0.0045 cm/cm0.0045 in/inrestricted
Melt Flow 92.25 g/10 min
@Load 5.00 kg,
Temperature 275 °C
92.25 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 70.0 MPa10200 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 15 %15 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 3.50 GPa508 ksiISO 527-1/-2
Flexural Strength 100 MPa14500 psiat max force; ISO 178
Flexural Modulus 2.50 GPa363 ksiISO 178
Charpy Impact Unnotched 10.5 J/cm²
@Temperature 23.0 °C
50.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2100 MPa
@Strain <=0.5 %
305000 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.24
@Frequency 1e+6 Hz
0.24
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.60 J/g-°C0.382 BTU/lb-°F
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 135 °C275 °Ffor 50% loss of tensile strength after 20000hr
 165 °C329 °Ffor 50% loss of tensile strength after 5000hr
 200 °C392 °F
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FInjection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection-molding
 
Descriptive Properties
Commercial StatusEurope and North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Custom Resins Nylene® 434 Un-reinforced Nylon 6
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry)
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned)

PBASG0256 / 131889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.