MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP Lexan® EXCP0076 Polycarbonate, 30% Glass Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Internal mold release.

  • Features: Good Mold Release, Flame Retardant, ECO Compliant
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccASTM D792
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 107 MPaType I, 5mm/min; ASTM D638
Tensile Strength, Yield 107 MPaType I, 5mm/min; ASTM D638
Elongation at Break 4.0 %Type I, 5mm/min; ASTM D638
Elongation at Yield 4.0 %Type I, 5mm/min; ASTM D638
Flexural Strength 149 MPa50.8 mm Span, 1 mm/min; ASTM D790
Flexural Modulus 9.65 GPa(50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched 0.534 J/cmASTM D256
Izod Impact, Unnotched 2.67 J/cmASTM D256
Falling Dart Impact 6.78 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Vicat Softening Point 98.9 °CRate B; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 277 °C
Middle Barrel Temperature 271 - 288 °C
Front Barrel Temperature 271 - 299 °C
Nozzle Temperature 271 - 299 °C
Melt Temperature 271 - 310 °C
Mold Temperature 48.9 - 93.3 °C
Drying Temperature 82.2 - 87.8 °C
Dry Time 3 - 8 hour
Back Pressure 0.345 - 0.689 MPa
Shot Size 40 - 60 %Suggested
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 35 - 75 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, 40% Glass Filled
Overview of materials for Nylon 46, Unreinforced
Overview of materials for Polypropylene, Molded
Kuraray Genestar™ G1350A-M42 Nylon, 35% Glass Filled
Aclo Accutech Polypropylene CP0409HUUVV Copolymer UV Stabilized

PZLNP1054 / 51136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.