MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Nikrothal 40 Resistance Wire
Categories: Metal; Superalloy; Iron Base

Material Notes: NIKROTHAL 40 is used as electric heating element material in domestic appliances and other electric heating equipment at operating temperatures up to 1100°C (2010°F). It has good ductility after use, good corrosion resistance except in sulphur containing atmospheres and certain controlled atmospheres and excellent weldability.

Typical applications for NIKROTHAL 40 are night-storage heaters, convection heaters, heavy duty rheostats and fan heaters. NIKROTHAL 40 is also used in heating cables and rope heaters in defrosting and de-icing elements, electric blankets and pads, car seats, baseboard heaters, floor heaters, resistors, etc.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160
@Thickness 4.00 mm
 180
@Thickness 1.00 mm
Tensile Strength, Ultimate 58.0 MPa
@Temperature 1000 °C
deformation rate= 5.0x10-2/min
 95.0 MPa
@Temperature 900 °C
deformation rate= 6.2x10-2/min
 170 MPa
@Temperature 800 °C
deformation rate= 5.0x10-2/min
 650 MPa
@Thickness 4.00 mm
 675 MPa
@Thickness 1.00 mm
Tensile Strength, Yield 300 MPa
@Strain 0.2 %,
Thickness 4.00 mm
 340 MPa
@Strain 0.2 %,
Thickness 1.00 mm
Elongation at Break 30 %
@Thickness 4.00 mm
 35 %
@Thickness 1.00 mm
Creep Strength 4.00 MPa
@Temperature 1000 °C,
Time 3.60e+6 sec
1% elongation
 20.0 MPa
@Temperature 800 °C,
Time 3.60e+6 sec
1% elongation
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000104 ohm-cm
 0.000107 ohm-cm
@Temperature 100 °C
 0.000110 ohm-cm
@Temperature 200 °C
 0.000114 ohm-cm
@Temperature 300 °C
 0.000116 ohm-cm
@Temperature 400 °C
 0.000119 ohm-cm
@Temperature 500 °C
 0.000121 ohm-cm
@Temperature 600 °C
 0.000123 ohm-cm
@Temperature 700 °C
 0.000125 ohm-cm
@Temperature 800 °C
 0.000126 ohm-cm
@Temperature 900 °C
 0.000128 ohm-cm
@Temperature 1000 °C
 0.000129 ohm-cm
@Temperature 1100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 250 °C
 17.0 µm/m-°C
@Temperature 20.0 - 500 °C
 18.0 µm/m-°C
@Temperature 20.0 - 750 °C
 19.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
 0.500 J/g-°C
@Temperature 100 °C
 0.500 J/g-°C
@Temperature 200 °C
 0.510 J/g-°C
@Temperature 300 °C
 0.540 J/g-°C
@Temperature 400 °C
 0.570 J/g-°C
@Temperature 500 °C
 0.600 J/g-°C
@Temperature 600 °C
 0.620 J/g-°C
@Temperature 700 °C
 0.640 J/g-°C
@Temperature 800 °C
 0.670 J/g-°C
@Temperature 900 °C
 0.700 J/g-°C
@Temperature 1000 °C
 0.730 J/g-°C
@Temperature 1100 °C
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 °C
 14.0 W/m-K
@Temperature 100 °C
 15.0 W/m-K
@Temperature 200 °C
 16.0 W/m-K
@Temperature 300 °C
 18.0 W/m-K
@Temperature 400 °C
 19.0 W/m-K
@Temperature 500 °C
 21.0 W/m-K
@Temperature 600 °C
 22.0 W/m-K
@Temperature 700 °C
 24.0 W/m-K
@Temperature 800 °C
 25.0 W/m-K
@Temperature 900 °C
 26.0 W/m-K
@Temperature 1000 °C
 28.0 W/m-K
@Temperature 1100 °C
Melting Point 1390 °C
Maximum Service Temperature, Air 1100 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.88fully oxidized
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Chromium, Cr 18 - 21 %
Iron, Fe >= 38.4 %
Manganese, Mn <= 1.0 %
Nickel, Ni 34 - 37 %
Silicon, Si 1.6 - 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV082 / 18976

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.