MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 8015 sec; ASTM D2240
Tensile Strength, Yield 42.3 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 3060 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPaASTM D790
Flexural Modulus 2660 MPaASTM D790
Izod Impact, Notched 120 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Compression Molded, all complete breaks; ASTM D256A
 880 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Compression Molded, all hinge breaks; ASTM D256A
 1200 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded, all hinge breaks; ASTM D256A
Dart Drop, Total Energy 19.8 J
@Thickness 1.85 mm,
Temperature -18.0 °C
brittle, 3.30 m/sec; ASTM D3763
 21.9 J
@Thickness 1.85 mm,
Temperature 0.000 °C
brittle, 3.30 m/sec; ASTM D3763
 25.1 J
@Thickness 1.85 mm,
Temperature 23.0 °C
ductile, 3.30 m/sec; ASTM D3763
Dart Drop Total Energy 66.7 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 >= 178 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 63.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.7 °CUnannealed; ASTM D648
 80.0 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CAnnealed; ASTM D648
 74.5 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.701 mm
ALL; UL 94
 5VA
@Thickness 3.00 mm
ALL; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 177 - 188 °C
 
Descriptive Properties
Agency RatingsNSF 51
 UL 94
Ease of SizingGood
FeaturesGood Surface Finish
 High Flow
FormsCube
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16364ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesProfiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 8266 Rigid PVC, Extrusion, Natural

PH0POL1057 / 145626

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.