MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Geon® Performance Solutions Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 808015 sec; ASTM D2240
Tensile Strength, Yield 42.3 MPa6140 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.06 GPa444 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.66 GPa386 ksiASTM D790
Izod Impact, Notched  1.20 J/cm
@Thickness 3.18 mm,
Temperature -18.0 °C
2.25 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
Compression Molded, all complete breaks; ASTM D256A
 8.80 J/cm
@Thickness 3.18 mm,
Temperature 0.000 °C
16.5 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
Compression Molded, all hinge breaks; ASTM D256A
 12.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
22.5 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, all hinge breaks; ASTM D256A
Dart Drop, Total Energy  19.8 J
@Thickness 1.85 mm,
Temperature -18.0 °C
14.6 ft-lb
@Thickness 0.0728 in,
Temperature -0.400 °F
brittle, 3.30 m/sec; ASTM D3763
 21.9 J
@Thickness 1.85 mm,
Temperature 0.000 °C
16.2 ft-lb
@Thickness 0.0728 in,
Temperature 32.0 °F
brittle, 3.30 m/sec; ASTM D3763
 25.1 J
@Thickness 1.85 mm,
Temperature 23.0 °C
18.5 ft-lb
@Thickness 0.0728 in,
Temperature 73.4 °F
ductile, 3.30 m/sec; ASTM D3763
Dart Drop Total Energy  66.7 J/cm
@Temperature 23.0 °C
0.125 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 >= 178 J/cm
@Temperature 23.0 °C
>= 0.333 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C35.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.7 °C172 °FUnannealed; ASTM D648
 80.0 °C176 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FAnnealed; ASTM D648
 74.5 °C
@Thickness 3.18 mm
166 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 0.701 mm
V-0
@Thickness 0.0276 in
ALL; UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 - 188 °C351 - 370 °F
 
Descriptive Properties
Agency RatingsNSF 51
 UL 94
Ease of SizingGood
FeaturesGood Surface Finish
 High Flow
FormsCube
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16364ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesProfiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 8266 Rigid PVC, Extrusion, Natural

PH0POL1057 / 145626

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.