System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 20% Glass Fiber Filled
Material Notes:
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire test up to 960 °C.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.500
-
0.800
g/cc
Density
1.31
g/cc
ISO 1183
Moisture Absorption at Equilibrium
2.0 - 2.4 %
23°C; 50% RH; ISO 62
Linear Mold Shrinkage
0.0060
cm/cm
Melt Flow
157.2
g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
50.0
MPa
50 mm/min; ISO 527-1/-2
Elongation at Yield
6.0 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity
3.00
GPa
ISO 527-1/-2
Charpy Impact Unnotched
110
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+11
ohm-cm
IEC 60093
Surface Resistance
1.00e+10
ohm
IEC 60093
Comparative Tracking Index
600
V
Test solution A; IEC 60112
Hot Wire Ignition, HWI
2.0
sec
@Thickness >=1.50 mm
ASTM D3874-88
High Amp Arc Ignition, HAI
0.00
arcs
@Thickness >=0.700 mm
UL 746C
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
>=
50.0
µin/in-°F
Melting Point
220
°C
ISO 3146
Decomposition Temperature
>=
300
°C
UL RTI, Electrical
140
°C
@Thickness 1.50 mm
UL 746B
Oxygen Index
29 %
ISO 4589-2
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
IEC 60695-2-12
Ignition Temperature
>=
350
°C
ASTM D1929
Descriptive Properties
Color
Grey 22985
Commercial Status
Europe
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Glass Fiber Filled
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned)
PBASG0397 / 132030
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.